Chemical Composition
0.15
%  (maximum)  
20.5 to 23.5
%    
59.3 to 69.5
%    (estimate)
2
%  (maximum)  
10 to 13
%    
0.03
%  (maximum)  
0.025
%  (maximum)  
2
%  (maximum)  
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 