Chemical Composition
0.025
%  (maximum)  
19 to 22
%    
45.7 to 58.4
%    (estimate)
5 to 9
%    
2.5 to 3.5
%    
0.15 to 0.2
%    
15 to 18
%    
0.035
%  (maximum)  
0.025
%  (maximum)  
1.5
%  (maximum)  
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 