Chemical Composition
0.025
%  (maximum)  
17 to 20
%    
49.4 to 60.5
%    (estimate)
2.5 to 5
%    
4 to 5
%    
16 to 19
%    
0.035
%  (maximum)  
0.025
%  (maximum)  
1.5
%  (maximum)  
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Other Information
Links
Organizations

 



No warranty is given for the accuracy of these data
Copyright © 2024 ASM International®