Chemical Composition
0.25
%  (maximum)  
15.5 to 18.5
%    
76.2 to 84
%    (estimate)
1.5
%  (maximum)  
0.5 to 1.5
%    
1
%  (maximum)  
0.03
%  (maximum)  
0.025
%  (maximum)  
1
%  (maximum)  
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 