Chemical Composition
0.1
%    
17
%    
82.5
%    (estimate)
0.2
%    
0.2
%    
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
345 to 379
MPa    
538 to 641
MPa    
18 to 20
% strain    
137 to 150
   
 
Other Information
Links
Organizations

 



No warranty is given for the accuracy of these data