Chemical Composition
0.28 to 0.55
%    
18 to 20
%    
63.2 to 70.6
%    (estimate)
0.7 to 1.5
%    
1 to 1.7
%    
0.4
%    
8 to 11
%    
1 to 1.7
%    
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
476
MPa    
58
% strain    
216
   
 
Other Information