Chemical Composition
0.22
%    
26.5
%    
50.1
%    (estimate)
1.8
%    
21
%    
0.4
%    
also 0.30 C, or 0.40 C
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 