Chemical Composition
0.07 to 0.17
%    
18 to 20.5
%    
63.8 to 69.6
%    (estimate)
3.3 to 4.75
%    
0.25
%  (maximum)  
9 to 10.5
%    
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
386 to 427
MPa    
579 to 662
MPa    
37 to 46
% strain    
 
Other Information
Links
Organizations

 