Chemical Composition
0.07
%  (maximum)  
18.5 to 21
%    
63.8 to 73
%    (estimate)
2
%  (maximum)  
1.1
%  (maximum)  
8.5 to 10.5
%    
0.03
%  (maximum)  
0.025
%  (maximum)  
1.5
%  (maximum)  
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 