Chemical Composition
0.51
%    
1.05
%    
96.5
%    (estimate)
0.97
%    
0.25
%    
0.53
%    
0.21
%    
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
1030
MPa    
1140
MPa    
20
% strain    
280 to 310
   
 
Other Information
Heat treated: 165,000 TS; 150,000 YS; 20 El; 59 RA; 280-310 HB; For arbors, axles, bolts, cams, gears, hubs, die liners; shock and fatigue resistant, preheat treated at mill.