Chemical Composition
0.35 to 0.45
%    
9 to 11
%    
83.4 to 87.9
%    (estimate)
0.8
%  (maximum)  
0.8 to 1.3
%    
0.04
%  (maximum)  
0.03
%  (maximum)  
2 to 3
%    
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 