Chemical Composition
0.03
%  (maximum)  
21 to 23
%    
63.7 to 71.9
%    (estimate)
2
%  (maximum)  
2.5 to 3.5
%    
0.08 to 0.2
%    
4.5 to 6.5
%    
0.03
%  (maximum)  
0.02
%  (maximum)  
1
%  (maximum)  
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 