Chemical Composition
0.12
%  (maximum)  
5.5 to 6.5
%    
89.8 to 92.5
%    (estimate)
1
%  (maximum)  
0.045
%  (maximum)  
0.03
%  (maximum)  
2 to 2.5
%    
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 