Chemical Composition
0.002
%  (maximum)  
0.015 to 0.03
%    
0.25
%  (maximum)  
17 to 18
%    
0.05
%  (maximum)  
63.8 to 67
%    (estimate)
1.6 to 2
%    
2.3 to 2.7
%    
0.06 to 0.08
%    
12 to 12.5
%    
0.035
%  (maximum)  
0.02
%  (maximum)  
0.5
%  (maximum)  
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 