Chemical Composition
0.05 to 0.2
%    
10.5 to 12.5
%    
68.3 to 75
%    (estimate)
5.5 to 6.5
%    
0.75
%  (maximum)  
0.1
%  (maximum)  
9 to 11
%    
0.6
%  (maximum)  
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
230
MPa    
530 to 730
MPa    
40
% strain    
 