Chemical Composition
0.03
%  (maximum)  
21.5 to 24
%    
55 to 62.1
%    (estimate)
1.2
%  (maximum)  
1.2 to 1.6
%    
0.25 to 0.4
%    
14 to 16
%    
0.03
%  (maximum)  
0.015
%  (maximum)  
1 to 1.7
%    