Chemical Composition
0.12
%  (maximum)  
17.5 to 20
%    
57.1 to 64.6
%    (estimate)
17.5 to 20
%    
0.4 to 0.7
%    
1
%  (maximum)  
0.06
%  (maximum)  
0.03
%  (maximum)  
1
%  (maximum)  
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 