Range attributes
0.53
%    
21
%    
65.3
%    (estimate)
9
%    
0.42
%    
3.75
%    
 
Discrete attributes
Short text attributes
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
USA
For valves and valve seats. SAE EV8.
AL TECH 21-4
 
Long text attributes
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
For valves and valve seats. SAE EV8.
 
Hyperlink attributes
Integer attributes
ID
60471
231893
 
Further Information



No warranty is given for the accuracy of these data