Chemical Composition
0.15
%    
15
%    
24.9
%    (estimate)
60
%    
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
241 to 345
MPa    
586 to 689
MPa    
25 to 35
% strain    
 
Other Information
Untreated: 85,000-100,000 TS; 35,000-50,000 YS; 35-25 El; 55-45 RA. For furnace parts, crucibles, autoclaves, recuperators; heat and corrosion resistant to 1150 C.