Chemical Composition
0.7 to 1.4
%    
98.1 to 98.8
%    (estimate)
0.25
%    
0.25
%    
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
56 to 60
   
 
Other Information
Typical heat treated hardness: 56-60 HRC; For threading dies, shear knives, chisels, drills, punches, trimming and blanking dies, cold heading dies, pneumatic tools. Water hardening. AISI W-1.