Coating (low-dilution weld deposit) alloy; Fe-base alloy containing C, Mn, Mo, Si, Co, Cr and Cb. Designed as a precipitation hardening iron-base alloy. For screws, reamers, stabilizers and blades. 58 HRC age hardened.