Chemical Composition
0.06
%    
8.57
%    
0.03
%    
89.2
%    (estimate)
0.75
%    
1.02
%    
0.017
%    
0.018
%    
0.32
%    
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
243
MPa    
36
% strain    
 
Other Information