Chemical Composition
0.0008 to 0.005
%    
0.32 to 0.4
%    
0.3 to 0.6
%    
97.6 to 98.8
%    (estimate)
0.6 to 0.9
%    
0.035
%  (maximum)  
0.035
%  (maximum)  
0.4
%  (maximum)  
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 