Chemical Composition
0.02 to 0.05
%    
0.17 to 0.23
%    
0.35 to 0.65
%    
0.25
%  (maximum)  
96.7 to 98.3
%    (estimate)
0.6 to 0.9
%    
0.15 to 0.25
%    
0.012
%  (maximum)  
0.4 to 0.7
%    
0.02
%  (maximum)  
0.02
%  (maximum)  
0.25
%  (maximum)  
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 