Chemical Composition
0.02
%  (minimum)  
0.19
%  (maximum)  
96.7 to 98.1
%    (estimate)
1.2 to 1.65
%    
0.02
%  (maximum)  
0.004
%  (maximum)  
0.5 to 0.85
%    
0.025
%  (maximum)  
0.015
%  (maximum)  
0.15 to 0.5
%    
0.02
%  (maximum)  
0.02
%  (maximum)  
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 