Chemical Composition
0.02 to 0.055
%    
0.015
%  (maximum)  
0.12 to 0.18
%    
0.15
%  (maximum)  
0.06
%  (maximum)  
96.6 to 98
%    (estimate)
1.2 to 1.65
%    
0.05
%  (maximum)  
0.015
%  (maximum)  
0.004
%  (maximum)  
0.5 to 0.85
%    
0.015
%  (maximum)  
0.005
%  (maximum)  
0.15 to 0.35
%    
0.01
%  (maximum)  
0.02
%  (maximum)  
0.02
%  (maximum)  
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 