Range attributes
0.4
%    
5.25
%    
91.4
%    (estimate)
1
%    
1
%    
1
%    
 
Logical attributes
Yes
 
Discrete attributes
Short text attributes
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
USA
General purpose hot work die steel for aluminum and zinc die casting dies, hot extrusion and forging; also cold heading and plastic molding. Air hardening. AISI H-13.
POTOMAC M
 
Long text attributes
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
General purpose hot work die steel for aluminum and zinc die casting dies, hot extrusion and forging; also cold heading and plastic molding. Air hardening. AISI H-13.
 
Hyperlink attributes
Integer attributes
ID
60637
231893
 
Further Information



No warranty is given for the accuracy of these data