Chemical Composition
0.45
%    
3.5
%    
81.5
%    (estimate)
0.6
%    
14
%    
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
1850 to 2140
MPa    
1 to 23
% strain    
321 to 600
   
 
Other Information
Oil hardened: 310,000-268,000 TS; 1-23 El; 5-79 RA; 600-321 HB; Heavy duty tungsten hot work tool steel suitable for hot shear blades, hot punches, long run hot forging and extrusion dies. AISI H-24.
MOHAWK HOT DIE
 
Links



No warranty is given for the accuracy of these data