Chemical Composition
0.25 to 0.3
%    
1 to 1.2
%    
94.3 to 95
%    (estimate)
0.2
%    
3.5 to 4
%    
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 