Chemical Composition
0.25
%  (maximum)  
55 to 58
%    
0.35
%  (maximum)  
2 to 3.5
%    
1.5 to 2.5
%    
0.25 to 1.5
%    
0.5 to 1.5
%    
32.4 to 40.8
%    (estimate)
Zn is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
379
MPa    
19
% strain    
 