Chemical Composition
1.45
%    
0.2
%    
96.2
%    (estimate)
0.8
%    
0.25
%    
1.15
%    
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
58 to 62
   
 
Other Information
Usual heat treated hardness: 58/62 HRC; Graphitic oil hardening tool steel of outstanding machinability. For blanking and forming dies, punches, gages, fixtures and machine parts. AISI O-6.