Chemical Composition
0.9
%    
0.08
%    
97
%    (estimate)
1.5
%    
0.3
%    
0.2
%    
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
58 to 62
   
 
Other Information
Links



No warranty is given for the accuracy of these data