Chemical Composition
0.85 to 1.2
%    
0.36
%    
1.49
%    
95.7 to 96.5
%    (estimate)
0.4 to 0.7
%    
0.18
%    
0.2 to 0.4
%    
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
586 to 1240
MPa    
717 to 1540
MPa    
11 to 18
% strain    
200 to 445
   
 
Other Information
Heat treated: 224,000-104,000 TS; 180,000-85,000 YS; 11-18 El; 36-59 445-200 HB; For nitrided gears, shafts, cams, clutches, rollers; nitriding steel.