Chemical Composition
0.95 to 1.20
%    
16.00 to 18.00
%    
77.5 to 83.1
%    (estimate)
1.00
%  (maximum)  
0.75
%  (maximum)  
0.50
%  (maximum)  
0.040
%  (maximum)  
0.030
%  (maximum)  
1.00
%  (maximum)  
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
483
MPa    
15
% strain    
 
Other Information
For bearings, bushings, valve components, cutlery and pump parts. High-hardening, outstanding wear resistance, good corrosion resistance. Bar, wire, billet, extruded rolled shape. Annealed: 110 ksi TS; 70 ksi YS; 15 EL; 98 HRC; 30 RA.