0.55
%    
0.9
%    
91.5
%    (estimate)
0.8
%    
0.5
%    
3.6
%    
2.1
%    
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
2360
MPa    
 