Chemical Composition
0.005
%  (maximum)  
0.2
%  (maximum)  
1
%  (maximum)  
0.5
%  (maximum)  
93.5 to 99.9
%    (estimate)
1.7
%  (maximum)  
0.6
%  (maximum)  
0.05
%  (maximum)  
1.5
%  (maximum)  
0.025
%  (maximum)  
0.025
%  (maximum)  
0.15 to 0.8
%    
0.12
%  (maximum)  
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 