Range attributes
330 to 400
   
0.45
%    
0.85
%    
95.7
%    (estimate)
0.75
%    
0.3
%    
2
%    
1240 to 1450
MPa    
1030 to 1240
MPa    
 
Logical attributes
Yes
Yes
 
Discrete attributes
Short text attributes
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
USA
Heat treated: 180,000-210,000 TS; 150,000-180,000 YP; 20-25 RA; 330-400 HB; For general and structural castings, shafts, gears, housings. AISI 4340. Shock resistant.
BIRDSBORO-40A3
 
Long text attributes
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
Heat treated: 180,000-210,000 TS; 150,000-180,000 YP; 20-25 RA; 330-400 HB; For general and structural castings, shafts, gears, housings. AISI 4340. Shock resistant.
 
Hyperlink attributes