Range attributes
301 to 550
   
0.65 to 0.75
%    
1.3 to 1.6
%    
95.2 to 95.8
%    (estimate)
0.35 to 0.45
%    
1.9 to 2
%    
 
Logical attributes
Yes
Yes
 
Discrete attributes
Short text attributes
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
USA
Cast: 301-550 HB; For castings, wear plates; wear resisting.
KISSOCK STEEL
 
Long text attributes
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
Cast: 301-550 HB; For castings, wear plates; wear resisting.
 