Chemical Composition
0.25
%    
25
%    
52.4
%    (estimate)
0.5
%    
20
%    
1.85
%    
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
276
MPa    
483 to 586
MPa    
10 to 75
% strain    
160 to 180
   
83 to 89
   
 
Other Information