Range attributes
1.5
%    
5
%    
4.7
%    
71.3
%    (estimate)
66 to 68
   
5
%    
12.5
%    
 
Discrete attributes
Short text attributes
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
USA
Usual heat treated hardness: 66-68 HRC; For heavy duty cutting tools requiring extra red hardness and abrasion resistance. W-C-Co high-speed steel. AISI T-15.
PANTHER 5
 
Long text attributes
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
Usual heat treated hardness: 66-68 HRC; For heavy duty cutting tools requiring extra red hardness and abrasion resistance. W-C-Co high-speed steel. AISI T-15.
 