Chemical Composition
0.86
%    
2.8
%    
4.3
%    
77.1
%    (estimate)
0.85
%    
2.1
%    
12
%    
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 