Chemical Composition
Mechanical Properties
 
Other Information
Silver solder type alloy for torch, furnace or induction brazing, ferrous and non-ferrous alloys. 1295 F MP; 58,000 psi TS.
FLOTECTIC SILVER 2
 
Links
Organizations

 



No warranty is given for the accuracy of these data