Chemical Composition
96.3
%    (estimate)
3.5
%    
0.25
%    
Al is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
260
MPa    
7
% strain    
 
Other Information
Links