Range attributes
0.7
%    
3.25 to 4.25
%    
82.5 to 86.6
%    (estimate)
7.5 to 9.5
%    
0.75 to 1
%    
1.2 to 2
%    
 
Discrete attributes
Short text attributes
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
USA
For reamers, lathe tools, drills, broaches; high-speed steel, oil hardened.
LUDLUM LMW-EZ
 
Long text attributes
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
For reamers, lathe tools, drills, broaches; high-speed steel, oil hardened.
 
Hyperlink attributes
Integer attributes
ID
60601
231893
 
Further Information