Chemical Composition
1.05 to 1.12
%    
7.5 to 8.5
%    
3.6 to 4.4
%    
72 to 76.7
%    (estimate)
0.4
%  (maximum)  
9 to 10
%    
0.03
%  (maximum)  
0.03
%  (maximum)  
0.45
%  (maximum)  
1 to 1.3
%    
1.2 to 1.8
%    
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 