Chemical Composition
0.92
%    
4.8
%    
4
%    
77.1
%    (estimate)
5
%    
1.9
%    
6.3
%    
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
240 to 300
   
 
Other Information
Links
Organizations

 