Chemical Composition
1.09
%    
8
%    
3.75
%    
83.9
%    (estimate)
0.2
%    
0.3
%    
1.15
%    
1.6
%    
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
67 to 70
   
 
Other Information
Usual heat-treated hardness: 67/70 HRC; Heavy duty high-speed steel designed to machine high temperature alloys, titanium, and prehardened alloy steels. AISI M42.