Range attributes
0.9
%    
2
%    
5
%    
78.4
%    (estimate)
1
%    
8.5
%    
0.7
%    
1
%    
2.5
%    
 
Discrete attributes
Short text attributes
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
USA
Welded: 60 HRC; For hardfacing electrodes; high-speed tool steel resistant to abrasion, oxidation, light impact to 1000 F.
DIAMEND 63
 
Long text attributes
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
Welded: 60 HRC; For hardfacing electrodes; high-speed tool steel resistant to abrasion, oxidation, light impact to 1000 F.
 