Chemical Composition
0.02
%  (minimum)  
0.0005
%  (minimum)  
0.1 to 0.2
%    
0.4 to 0.65
%    
0.15 to 0.5
%    
95.6 to 97.4
%    (estimate)
0.6 to 1
%    
0.4 to 0.6
%    
0.7 to 1
%    
0.025
%  (maximum)  
0.025
%  (maximum)  
0.15 to 0.35
%    
0.03 to 0.08
%    
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 