Chemical Composition
0.05 to 0.15
%    
0.005
%  (maximum)  
0.03
%  (maximum)  
8 to 10
%    
64.3 to 70
%    (estimate)
0.1
%  (maximum)  
4.5 to 5.5
%    
17 to 19
%    
0.01
%  (maximum)  
0.01
%  (maximum)  
0.1
%  (maximum)  
0.5 to 0.8
%    
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 